Ejection System Design for LSR: Ejector Pins, Air Valves and Undercuts
Overview: Liquid silicone parts are soft, easily deformed and high in friction, which makes demolding far harder than with a rigid plastic. Poor design tears the part, leaves ejector marks, jams it in the tool, or damages the tool itself. A sensible ejection system is therefore a combination of mechanical ejection, air ejection and auxiliary aids, chosen to suit the part structure.
What Makes Demolding Hard
Silicone has a high coefficient of friction, roughly 0.5 to 1.0 against steel against 0.2 to 0.3 for a rigid plastic, and the part is too soft to take concentrated ejection force. Apply rigid-plastic ejection logic to silicone and the usual result is a pin pushing straight through the part, or severe distortion once it is out.
There is also a suction effect. The smoother the cavity surface, the more easily negative pressure builds between part and cavity, and deep, thin-wall parts in particular need a considerable force to overcome that suction at ejection.
Choosing an Ejection Method
Mechanical ejector pins suit products with enough rigidity and a large ejection area. A pin diameter of 2 to 4 mm is recommended, with the ejection area spread as widely as possible to avoid concentrated stress. Pin faces should be machined spherical or fitted with a silicone pad, to increase contact area.
Air ejection, using an air valve, is the most elegant solution for silicone: a venting-style air valve set into the core with a gap of 0.02 to 0.05 mm admits compressed air at 3 to 6 bar, forming an air film between part and core that lifts the part out evenly. The advantages are no ejector marks and uniform loading, which suits thin-wall, deep-cavity and cosmetic parts especially well. The disadvantages are a more complex structure, higher cost and tight machining requirements on the valve.

Handling Undercuts
One of the biggest advantages of LSR is that the material is soft enough to permit a degree of forced ejection. As a rule of thumb, silicone at 30 to 50 Shore A tolerates 5 to 10 percent forced deformation: where an undercut is no deeper than 10 percent of the local wall thickness and has no sharp edge, the part can simply be stripped off.
Beyond that, structural solutions are needed: a slide for side core pulling, a lifter for internal core pulling, or a split insert removed by hand after opening. Where a deep undercut is unavoidable, two-shot molding is worth considering — overmold the main body first, then complete the undercut in a second tool.
Draft and Surface Finish
Draft is recommended at 1 to 3 degrees per side: 1 to 1.5 degrees for a polished surface, plus 1 degree for every 0.025 mm of texture depth on a textured face. Deep cavities, more than 30 mm deep, should go above 3 degrees. Cavity surfaces are polished along the ejection direction; transverse marks are strictly forbidden, because transverse polish lines catch the part like a barb.
Auxiliary measures include fine bead blasting of the cavity, Ra 0.8 to 1.6 micrometres, to reduce adhesion; a semi-permanent release coating; and synchronized robot pick-up timed with ejection. Zhongshan Henry Precision Technology Co., Ltd. (Henry Precision) uses air ejection plus synchronized robot take-out as standard on deep-cavity, thin-wall overmolded parts, holding demolding yield stably above 99 percent.

Table of Contents
Related News
-
Tooling Essentials for LSR Precision Overmolding: Gate, Venting and Parting Line
Technical ArticlesLearn More -
Precision Tooling for LSR Overmolding: Cold Runner, Cavity and Demolding, End to End
Technical ArticlesLearn More -
Thin-Wall LSR Overmolding: Molding Difficulties and How to Solve Them
Technical ArticlesLearn More