Gate Design
The gate is the first decision in tooling for liquid silicone precision overmolding. LSR has low viscosity and pronounced shear thinning, so a pin-valve cold runner gate or an open pinpoint gate is the preferred choice, with gate diameter normally held between 0.3 and 0.8 mm. Too large and it leaves a visible gate mark and extra trimming work; too small and it causes short shots and shear overheating. In overmolded designs the gate also has to sit away from the substrate bond face and any cosmetic surface, so the melt does not wash directly over a pre-placed insert and shift it by 0.05 mm or more. The cold runner should be held at a constant 20 to 30 degrees Celsius to keep the compound from curing in the runner, with runner balance calculated so fill time varies by less than 0.2 seconds between cavities — that is the basis of cavity-to-cavity consistency.

Venting Layout
Liquid silicone flows extremely well and traps air just as easily; bubbles are one of the most common reasons for scrapping an overmolded part. The established approach is vacuum-assisted venting at the parting line: close the tool, draw a vacuum, and only start injection once the cavity reaches minus 0.09 megapascals or better. That step alone takes the bubble defect rate from over 3 percent down to under 0.3 percent. Vent groove depth has to be held strictly between 0.005 and 0.01 mm, because under injection pressure LSR will find its way into any gap wider than 0.02 mm and turn into flash. Venting goes where the melt front ends and along the edge where the insert sits; where needed, porous steel or venting inserts are added at insert joints. Process stability in liquid silicone overmolding depends heavily on how well the venting system is matched to injection speed.
Choosing the Parting Line
The parting line decides where flash appears and what appearance grade the part achieves. Three rules apply. Keep the parting line off sealing faces and customer-visible surfaces, so the flash line falls on an edge or a non-critical area. Match the insert placement direction to the parting line, so the part releases cleanly without tearing the silicone. Leave a sealing land on shut-off and interlocking features: hold shut-off flatness within 0.005 mm, keep interlocking draft at 3 degrees or more, and maintain 3 to 5 mm of engagement, so the tool does not leak under injection pressure. For medical overmolded parts, parting line roughness should stay below Ra 0.4 micrometres, to reduce flash residue.

Mold Temperature and Structural Accuracy
LSR cures with heat, so mold temperature is normally set between 170 and 200 degrees Celsius, with the difference between moving and fixed halves kept within plus or minus 5 degrees to avoid local overcure or undercure. Corrosion-resistant steels such as S136 or 718H are recommended, so catalyst residue from the platinum cure system does not attack the cavity. Moving fits are designed to H7/g6, and ejection systems get self-lubricating treatment. A qualified LSR precision overmolding tool should have mold flow analysis completed at the design stage, verifying fill balance, venting paths and predicted cure time. Zhongshan Henry Precision Technology Co., Ltd. (Henry Precision) brings mold flow simulation and DFM review into the tooling development stage, resolving gate, venting and parting line risks up front and cutting average production ramp-up time by more than 30 percent — reliable tooling engineering support for customers' liquid silicone precision overmolding projects.
Table of Contents
Related News
-
Defects in LSR Precision Overmolding: Bubbles, Flash, Sink Marks and Short Shots
Technical ArticlesLearn More -
Dimensional Tolerance in LSR Precision Overmolding: How Micron-Level Accuracy Is Achieved
Technical ArticlesLearn More -
Cleanroom Processing for LSR Precision Overmolding: Environmental Control and Contamination Prevention
Technical ArticlesLearn More