LSR Precision Overmolding Injection Parameters: Temperature, Pressure and Curing Time
1. Molding Process Challenges
Injection molding liquid silicone (LSR) differs fundamentally from molding conventional thermoplastics. Thermoplastics form by heating to melt and cooling to solidify, while liquid silicone is a two-component platinum-catalyzed addition system: the A and B components are mixed, then crosslink and cure inside the tool — a thermoset process. That single characteristic is why LSR molding is so sensitive to its three main parameters, heat, pressure and time. Too much heat and the compound cures early, scorching and blocking the runner; too little and it stays under-cured and tacky. Pressure imbalance produces flash and short shots. Bad timing hits cycle time and part performance directly. Knowing how to optimize these parameters is therefore what secures both quality and efficiency in liquid silicone precision overmolding.
2. Temperature Control
Temperature is the single most important control variable in LSR molding, and it runs through three stages, barrel, runner and tool. The barrel and metering system normally sit in a low band of 18 to 25 degrees Celsius, keeping the A and B components stable and stopping them crosslinking early. The cold runner is cooled to around 20 degrees too, so the silicone stays liquid until it enters the cavity. Mold temperature is what sets the cure rate, generally between 120 and 200 degrees, depending on wall thickness and cure chemistry. Thin-wall precision parts typically run 170 to 190 degrees to shorten cycle time, while thick sections run cooler, so the surface does not over-cure while the core stays under-cured. Henry Precision uses independently zoned temperature control and thermal imaging on the floor to hold cavity temperature uniformity within plus or minus 3 degrees, which is what keeps cure level consistent and dimensions stable across precision overmolded parts.

Figure 1 Multi-zone temperature control system on an LSR injection molding machine
3. Pressure and Speed
LSR has low viscosity and flows easily, roughly 10 to 1,000 pascal-seconds, so injection pressure runs far below thermoplastics; 5 to 50 megapascals usually fills the cavity. What matters is how pressure is matched to speed. Inject too fast and you entrain air and get bubbles; too slow and the compound cures in the runner, causing short shots or cold material. Too little injection pressure leaves the far end unfilled; too much makes flash worse, and that shows up most clearly on the 0.3 mm-scale sealing lips typical of precision overmolding. The usual answer is a slow-fast-slow multi-stage injection profile with sensible holding and back pressure, keeping the cavity filled while cutting both overflow and molded-in stress.

Figure 2 Flow front and sealing lip as liquid silicone fills a precision cavity
4. Curing Time Control
Cure time sets the production takt and the properties the part ends up with. How fast LSR cures comes down to temperature, platinum catalyst loading and wall thickness together: a thin-wall part at 180 degrees Celsius demolds in seconds, while a thick or complex part needs tens of seconds or longer. Under-curing leaves poor rebound, high compression set and a tendency to bleed low-molecular-weight species; over-curing makes the part brittle and darkens its colour. To hold properties steady, precision parts usually get a second cure, post-curing, after demolding, which strips residual volatiles, completes the crosslink network, and lifts both mechanical and temperature performance. Setting cure time properly takes cure-curve trials and DSC testing, so you land on the best combination of in-mold cure and post-cure.

Figure 3 Cross-section of self-adhesive silicone bonded to a stainless steel substrate
5. Henry Precision
Zhongshan Henry Precision Technology Co., Ltd. works deep in liquid silicone precision overmolding, and has built a full-process parameter control system covering barrel, cold runner, tooling and post-cure. Backed by precision tooling, platinum-catalyzed molding and micron-level process control, Henry Precision can tailor a temperature, pressure, speed and cure time combination to each part's structure, wall thickness and performance requirements — treating precision as its foundation and making sure every overmolded part reaches a consistently high standard of dimensional accuracy, mechanical performance and weathering resistance.
Table of Contents
Related News
-
Designing an Automated LSR Overmolding Line: Flexible Tool Change in Practice
Technical ArticlesLearn More -
LSR Grades and Shore Hardness: A Selection Guide from Food Contact to Medical
Technical ArticlesLearn More -
What Governs Bond Strength in LSR Overmolding, and How to Control It
Technical ArticlesLearn More