Overview: with low viscosity and excellent flow, liquid silicone has a clear advantage in micro parts: wall thickness down to 0.15-0.2 mm and individual part weights as low as 0.01 g, with micro seals, light guides, keypad pads and sensor encapsulation all proven in production. But the difficulty with micro parts is not the molding — it is gating, demolding and inspection.



Where the Lower Limit Sits


From a production standpoint, the practical window for LSR micro parts is roughly: wall thickness 0.15-0.25 mm (below 0.15 mm needs a special low-viscosity grade and a vacuum cavity), part weight 0.01-0.5 g, and outer dimensions below 1 mm. A micro O-ring at 0.3 mm cross-section and a micro keypad pad at 1.5 mm diameter are both mature processes.


The limiting factor is mainly filling: the thinner the wall, the greater the flow resistance in the cavity, and heat is lost faster so the flow front cures prematurely. Low-viscosity grades (1,000-5,000 mPa·s) suit micro parts better than general-purpose grades.


Dimensional capability limits for liquid silicone micro parts


Gating Is the Hard Part


The most awkward part of a micro component is the gate. The part itself may weigh only 0.02 g, while the gate and runner often weigh more than the part — material utilization is poor; make the gate too small and you get short shots or shear overheating. In practice, pinpoint gates (0.2-0.4 mm diameter) or submarine gates are used, combined with a cold runner system to keep runner scrap to a minimum.


For extremely small parts, a multi-cavity array (32-up, 64-up) can spread the cost per part, but this places high demands on tool machining accuracy and runner balance — fill time variation between cavities has to be held within 3%.


Demolding and Handling


Micro silicone parts are soft and light, and tend to stick to the core or fly off through static attraction during demolding. Common countermeasures: mirror polish the cavity to reduce adhesion, add air ejection to assist demolding, use a robot with vacuum suction for part removal, and ionised air where needed to eliminate static.


Draft angle matters more on micro parts: we recommend 1°-3° per side, with uniform surface roughness on the core to avoid local undercuts that tear thin walls.


Demolding and part removal for micro liquid silicone parts


How to Inspect


Callipers are not accurate enough for micro parts; dimensions need a vision measuring system (2D optical) or an optical microscope, with SPC on critical dimensions. Appearance checks use 10-20x magnification or automated optical inspection (AOI), looking mainly for short shots, flash and bubbles.


Because each part is low in value but high in volume, the inspection strategy is usually full first-article dimensioning plus in-process sampling plus periodic full inspection, rather than 100% inspection. Zhongshan Henry Precision Technology Co., Ltd. (Henry Precision) runs vision systems and AOI on micro LSR parts and can carry out sampling plans to customer AQL standards.

Table of Contents

Get Your Custom Liquid Silicone Overmolding Solution in 3 Steps

Get Your Custom Liquid Silicone Overmolding Solution in 3 Steps

Learn More

We use cookies to personalize and improve your browsing experience. By clicking "Accept All", you consent to our use of cookies.
You may read our Cookie Policy for details.

A Leader in Precision LSR Overmolding

A Leader in Precision LSR Overmolding

Professional Consultation Services
We patiently answer your questions and resolve your concerns
+86 189 2812 0729 (24/7)<br>+86 136 9169 4353 (Sales - Mr. Lu) +86 189 2812 0729 (24/7)
+86 136 9169 4353 (Sales - Mr. Lu)
sales@henry-precision.com sales@henry-precision.com
*Your Name
*Your phone
Your email
Company name
*Requirements
Country / Region
*Special Requirements

We use this information solely to contact you regarding potential cooperation.
By submitting, you agree to our Privacy Policy。

Rubber Coating Requirement Assessment

Please complete the following information so that we can provide you with the evaluation result.

*Your name
*Your phone
Upload the drawings

Size should not exceed 5M and support. Doc,.Docx,.Pdf

Yuanheng guarantees that the collection of your personal information is solely for the purpose of contacting you and helping you better understand us.
By sending this message, you are agreeing to our "Privacy Policy" and "Disclaimer".