Engine Oil Seal
FKM Precision Overmolding Solution Engine Oil Seal
FKM Precision Overmolding Solution

Engine Oil Seal
FKM Precision Overmolding Solution

FKM overmolded onto the metal frame in one shot: withstands long-term immersion in gear and motor oils, stays stable across a wide temperature range without swelling, no debonding or edge lift in oil service, with an appearance step of ≤0.05 mm.
FKM Overmolding FKM + Metal Engine Oil Seal Oil-Resistant Seal Wide Temperature Range

Customer Requirements

The customer needed an oil seal for an engine powertrain: FKM overmolded onto a metal frame in one molding cycle, with reliable sealing, strong adhesion and a refined appearance under long-term oil immersion and thermal cycling.
FKM Overmolding FKM + Metal Engine Oil Seal Oil-Resistant Seal Wide Temperature Range
  • No swelling or leakage in long-term oil immersion
    No swelling or leakage in long-term oil immersion
    No debonding in hot and cold oil immersion
    No debonding in hot and cold oil immersion
  • No cracking under high-temperature aging
    No cracking under high-temperature aging
  • Flawless appearance with precise step tolerance
    Flawless appearance with precise step tolerance
    Passed alcohol immersion and assembly testing
    Passed alcohol immersion and assembly testing
  • Adopting <span>FKM-to-metal one-shot overmolding</span> to secure both sealing performance and frame strength Adopting <span>FKM-to-metal one-shot overmolding</span> to secure both sealing performance and frame strength
  • Henry Precision <span>in-house substrate pretreatment and curing process</span> eliminates false bonding Henry Precision <span>in-house substrate pretreatment and curing process</span> eliminates false bonding
  • Optimized <span>micro-anchor structuring</span> improves FKM-to-metal adhesion Optimized <span>micro-anchor structuring</span> improves FKM-to-metal adhesion
  • A <span>multi-stage validation system</span> covering appearance and oil resistance safeguards mass-production stability A <span>multi-stage validation system</span> covering appearance and oil resistance safeguards mass-production stability

The Solution

  • Adopting FKM-to-metal one-shot overmolding to secure both sealing performance and frame strength
    01
  • Henry Precision in-house substrate pretreatment and curing process eliminates false bonding
    02
  • Optimized micro-anchor structuring improves FKM-to-metal adhesion
    03
  • A multi-stage validation system covering appearance and oil resistance safeguards mass-production stability
    04

Henry Precision Highlights

Proven experience overmolding FKM onto multiple substrate types
Proven experience overmolding FKM onto multiple substrate types
In-house substrate pretreatment and post-molding curing process
In-house substrate pretreatment and post-molding curing process
Micro-anchor structuring for stronger bond strength
Micro-anchor structuring for stronger bond strength
Multi-stage appearance and oil-resistance validation before mass production
Multi-stage appearance and oil-resistance validation before mass production
  • Sealed with no leakage or swelling in oil immersion Sealed with no leakage or swelling in oil immersion
  • No debonding after alcohol immersion and assembly testing No debonding after alcohol immersion and assembly testing
  • Overmolding step measured with ≤0.05 mm precision Overmolding step measured with ≤0.05 mm precision
  • 100% appearance inspection - no flaws, flash or stains 100% appearance inspection - no flaws, flash or stains
  • Stable performance after thermal cycling Stable performance after thermal cycling

Key Validation

  • Oil-proof
    Sealed with no leakage or swelling in oil immersion
    Oil immersion test
  • Secure bond
    No debonding after alcohol immersion and assembly testing
    Alcohol test
  • ≤0.05mm
    Overmolding step measured with ≤0.05 mm precision
    Dimensional inspection
  • Consistent
    100% appearance inspection - no flaws, flash or stains
    Appearance inspection
  • Reliable
    Stable performance after thermal cycling
    Aging test
Get Your Custom Liquid Silicone Overmolding Solution in 3 Steps

Get Your Custom Liquid Silicone Overmolding Solution in 3 Steps

Learn More

We use cookies to personalize and improve your browsing experience. By clicking "Accept All", you consent to our use of cookies.
You may read our Cookie Policy for details.

A Leader in Precision LSR Overmolding

A Leader in Precision LSR Overmolding

Professional Consultation Services
We patiently answer your questions and resolve your concerns
+86 189 2812 0729 (24/7)<br>+86 136 9169 4353 (Sales - Mr. Lu) +86 189 2812 0729 (24/7)
+86 136 9169 4353 (Sales - Mr. Lu)
sales@henry-precision.com sales@henry-precision.com
*Your Name
*Your phone
Your email
Company name
*Requirements
Country / Region
*Special Requirements

We use this information solely to contact you regarding potential cooperation.
By submitting, you agree to our Privacy Policy。

Rubber Coating Requirement Assessment

Please complete the following information so that we can provide you with the evaluation result.

*Your name
*Your phone
Upload the drawings

Size should not exceed 5M and support. Doc,.Docx,.Pdf

Yuanheng guarantees that the collection of your personal information is solely for the purpose of contacting you and helping you better understand us.
By sending this message, you are agreeing to our "Privacy Policy" and "Disclaimer".