What Is the Minimum LSR Wall Thickness, and What Are the Risks?
Under ideal conditions the LSR overmold layer can be held to around 0.1–0.3 mm. But ultra-thin overmolding places extreme demands on tool vacuum, gate layout, injection parameters and insert positioning, and is prone to short shots, air traps, thickness variation and unfilled areas. A layer that is too thin also reduces tear resistance, aging resistance and sealing performance, so a DFM review at the design stage is necessary — pushing thickness to the absolute limit is not advisable.